MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Envalior Durethan® AKV 30 H2.0 901510 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: PA 66, 30% glass fibers, injection molding, heat-aging stabilized

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 g/cc0.0253 lb/in³ISO 60
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.0 %2.0 %50% RH; ISO 62
Water Absorption at Saturation 5.5 %5.5 %ISO 62
Linear Mold Shrinkage, Flow 0.0039 cm/cm0.0039 in/in60x60x2; 290 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0093 cm/cm0.0093 in/in60x60x2; 290 °C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance  800 N
@Temperature -30.0 °C
180 lb (f)
@Temperature -22.0 °F
ISO 6603-2
 900 N
@Temperature 23.0 °C
202 lb (f)
@Temperature 73.4 °F
ISO 6603-2
Ball Indentation Hardness 220 MPa31900 psiISO 2093-1
Tensile Strength at Break 175 MPa25400 psi5 mm/min; ISO 527-1,-2
Elongation at Break 3.0 %3.0 %5 mm/min; ISO 527-1,-2
 4.4 %4.4 %50 mm/min, Nominal; ISO 527-1,-2
Tensile Modulus 10.0 GPa1450 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 270 MPa39200 psi2 mm/min; ISO 178-A
Flexural Yield Strength 265 MPa
@Strain 3.5 %
38400 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 9.20 GPa1330 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 4.0 %4.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  <= 10.0 kJ/m²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  55.0 kJ/m²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 60.0 kJ/m²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched  6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 7.50 J/cm²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched  <= 1.00 J/cm²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
 <= 1.00 J/cm²
@Temperature -40.0 °C
<= 4.76 ft-lb/in²
@Temperature -40.0 °F
ISO 179 1eA
Puncture Energy  2.30 J
@Temperature -30.0 °C
1.70 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 2.80 J
@Temperature 23.0 °C
2.07 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant  4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250
 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
889 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.012
@Frequency 100 Hz
0.012
@Frequency 100 Hz
IEC 60250
 0.019
@Frequency 1e+6 Hz
0.019
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 475 V475 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
16.7 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 263 °C505 °F10°C/min; ISO 11357-1,-3
Maximum Service Temperature, Air 253 °C487 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FISO 75-1,-2
Vicat Softening Point  >= 230 °C
@Load 5.10 kg
>= 446 °F
@Load 11.2 lb
120°C/h; ISO 306
 >= 230 °C
@Load 5.10 kg
>= 446 °F
@Load 11.2 lb
50°C/h; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Oxygen Index 23 %23 %Method A; ISO 4589-2
Glow Wire Flammability Index  700 °C
@Thickness 0.800 mm
1290 °F
@Thickness 0.0315 in
IEC 60695-2-12
 700 °C
@Thickness 1.60 mm
1290 °F
@Thickness 0.0630 in
IEC 60695-2-12
 700 °C
@Thickness 3.00 mm
1290 °F
@Thickness 0.118 in
IEC 60695-2-12
Shrinkage, MD 0.070 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.070 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Flow Direction Post-Molding, 60x60x2; ISO 294-4
Shrinkage, TD 0.13 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.13 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Molding, 60x60x2; ISO 294-4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 °C554 °Finjection molding; ISO 294
 280 - 300 °C536 - 572 °F
Mold Temperature 80.0 °C176 °Finjection molding; ISO 294
 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 6.00 hour2.00 - 6.00 hour
Moisture Content 0.030 - 0.12 %0.030 - 0.12 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® AKV 30 H3.0 000000 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® AKV 30 000000 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® AKV 30 H2.0 901510 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® AKV 30 GIT H2.0 900116 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry

PLANW9220 / 208017

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.