MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik VESTAMID® L-GF30 black E70285 Nylon 12, 30% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 30% Glass Fiber Filled

Material Notes: VESTAMID® L-GF30 black E70285 is a glass fiber reinforced, heat-stabilized PA 12 compound with good IR laser transparency for injection molding. The material contains about 30% glass fibers, an ageing protective agent and processing aid for a fast and even form filling. VESTAMID® L-GF30 black E70285 is laser-wieldable by a diode-pumped or solid-state laser in the range of ? = 808–1064 nm. Using glass fiber reinforcement the strength and the heat deflection temperature are significantly increased. Further advantages of VESTAMID® L-GF30 black E70285 are the characteristic properties of polyamide 12 as low water absorption, good dimensional stability and almost the same properties at changing ambient humidity. VESTAMID® L-GF30 black E70285 is supplied as cylindrical pellets ready for processing in moisture-proof bags. Pigmentation may affect values.

Property data for dry samples unless otherwise noted.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4, 2577
Melt Flow 11 g/10 min
@Load 5.00 kg,
Temperature 250 °C
11 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psiISO 527
Tensile Strength, Yield 122 MPa17700 psiISO 527
Elongation at Break 6.0 %6.0 %ISO 527
Elongation at Yield 5.0 %5.0 %ISO 527
Tensile Modulus 6.80 GPa986 ksiISO 527
Charpy Impact Unnotched  8.50 J/cm²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eU
 10.0 J/cm²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
Complete Break, Conditioned; ISO 179/1eU
Charpy Impact, Notched  2.10 J/cm²
@Temperature -30.0 °C
9.99 ft-lb/in²
@Temperature -22.0 °F
Complete Break; ISO 179/1eA
 2.30 J/cm²
@Temperature 23.0 °C
10.9 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 175 °C347 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 165 °C329 °FISO 75-1/-2
Vicat Softening Point 175 °C347 °FMethod A: 10 N, 50 K/h; ISO 306
 175 °C347 °FMethod B: 10 N, 50 K/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Mold Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK843 / 243052

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.