MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPE EE-2250B Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink EE-2200 Series is a general purpose thermoplastic elastomer series, available in BLK, designed for automotive exterior extrusion applications. Sarlink EE-2250B is a medium hardness, high density, UV stabilized grade with very good extrudability.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: UV Stabilizer

Features: Good Adhesion; Good Flexibility; Good Processability; Good Toughness; High Density; High Specific Gravity; Medium Hardness; Ozone Resistant; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Viscosity 242 cP
@Shear Rate 206 1/s,
Temperature 200 °C
242 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.40 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5353ISO 868
 50
@Time 15.0 sec
50
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 4.52 MPa656 psiFlow; ISO 37
 6.86 MPa995 psiAcross Flow; ISO 37
Tensile Stress at Strain  1.17 MPa
@Strain 100 %
170 psi
@Strain 100 %
Across Flow; ISO 37
 1.76 MPa
@Strain 100 %
255 psi
@Strain 100 %
Flow; ISO 37
Elongation at Break 690 %690 %Flow; ISO 37
 870 %870 %Across Flow; ISO 37
Tear Strength 24.5 kN/m140 pliAcross Flow; ISO 34-1
Compression Set  15 %
@Temperature 22.8 °C,
Time 79200 sec
15 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 30 %
@Temperature 70.0 °C,
Time 79200 sec
30 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 76 %
@Temperature 125 °C,
Time 252000 sec
76 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Zone 1 193 - 204 °C380 - 400 °F
Zone 2 199 - 210 °C390 - 410 °F
Zone 3 204 - 216 °C400 - 420 °F
Zone 4 210 - 221 °C410 - 430 °F
Zone 5 210 - 221 °C410 - 430 °F
Die Temperature 216 - 227 °C420 - 440 °F
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
Teknor Apex Sarlink® TPE OM-1150N Thermoplastic Elastomer
Teknor Apex Sarlink® TPE ML-1650N NAT Thermoplastic Elastomer
Teknor Apex Sarlink® TPE ML-1150N NAT Thermoplastic Elastomer
Teknor Apex Sarlink® TPE ME-2350B BLK Thermoplastic Elastomer

PTEKNQ1027 / 237518

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.