MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Supreme Petrochem SC 203 LV General Purpose Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: Characteristics
  • Good flow grade with good mechanical properties
  • Good clarity and flexibility
  • Easy processing grade and suitable for thin walled applications
Processing
  • Extrusion
  • Molding
Applications
  • Suitable for glossy cap layer on HIPS in refrigerator industry
  • Suitable for tooth brushes and tooth brush containers, novelties, house wares and crystal wares
  • Ball pen barrels and geometric Instruments
Material Status: Commercial : Active

Agency Ratings: FDA 21 CFR 177.1640

Information provided by Supreme Petrochem LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 46.1 MPa50 mm/min; ASTM D638
Elongation at Break 2.0 %50 mm/min; ASTM D638
Flexural Strength 76.5 MPa
@Thickness 3.20 mm
ASTM D790
Flexural Modulus 29000 kg(f)/cm²
@Thickness 3.20 mm
ASTM D790
Izod Impact, Notched 20.0 J/m
@Thickness 3.20 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °CASTM D648
Vicat Softening Point 96.0 °C1kg load; 120°C/h; ASTM D1525
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 260 °C
Mold Temperature 40.0 - 60.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Supreme Petrochem SC 208 General Purpose Polystyrene
Supreme Petrochem SC 206 General Purpose Polystyrene
Resirene Resirene® HF-777 General Purpose Polystyrene
Supreme Petrochem SC 202EL General Purpose Polystyrene
Supreme Petrochem SC 201LV General Purpose Polystyrene

PSUP05 / 69437

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.