MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik Rohacell® 71 EC Electrically Conductive Grade Polymethacrylimide (PMI) Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polymethacrylimide

Material Notes: ROHACELL® EC is a polymethacrylimide (PMI) based foam core material specifically designed for stealth applications. During processing, the polymer is loaded with carbon particles resulting in a conductive foam product that possesses superior dielectric properties and enables absorption of electromagnetic waves at radar frequencies.

Due to its closed cell structure, ROHACELL® EC provides controlled resin absorption since the resin enters only the cut cells on the surface of the core material. This assures secure bonding of the core to the surface layers, but adds no excessive resin weight to the finished part.

Replaces Rohacell® 71EC-5.

Information provided by Evonik Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0750 g/cc0.00271 lb/in³DIN 53420, ISO 845, ASTM D 1622
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 2.00 MPa290 psiDIN 53455, ISO 527-2, ASTM D 638
Elongation at Break 3.2 %3.2 %ISO 527-2, ASTM D638
Modulus of Elasticity 0.105 GPa15.2 ksiISO 527-2, ASTM D 638
Compressive Strength 1.60 MPa232 psiDIN 53421, ISO 844, ASTM D 1621
Poissons Ratio 0.460.46Calculated
Shear Modulus 0.0360 GPa5.22 ksiDIN 53294, ASTM C 273
Shear Strength 1.00 MPa145 psiDIN 53294, ASTM C 273

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROHA31a / 287705

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.