MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ineos ABS Triax® 3158 ABS + Polyamide Blend (DAM), PA66/ABS Pellets (filled)  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend; Nylon (Polyamide PA)

Material Notes: Triax® 3158 is a PA+ABS-Blend and on-line paintable (195°C). It has very high heat resistance, reduced moisture, improved impact strength, and a low coefficient of linear thermal expansion. It is used for the production of molded plastic articles.

Triax® is now a INEOS Styrolution trade name; this grade is discontinued. Information provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Filler Content 9 %9 %Glass fiber / glass bead; ISO 3451-1
Linear Mold Shrinkage, Flow 0.011 cm/cm0.011 in/inTest Condition: 150x105x3; 280°C/MT 80°C; 500 bar; acc. ISO 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inTest Condition: 150x105x3; 280°C/MT 80°C; 500 bar; acc. ISO 2577
Melt Flow 10 g/10 min
@Load 10.0 kg,
Temperature 280 °C
10 g/10 min
@Load 22.0 lb,
Temperature 536 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 55.0 MPa7980 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 10 %>= 10 %50 mm/min; ISO 527-1,-2
 >= 10 %>= 10 %50 mm/min, Nominal; ISO 527-1,-2
Elongation at Yield 3.0 %3.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.90 GPa421 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 50.0 MPa7250 psi2 mm/min, @ 3.5% strain; ISO 178
 88.0 MPa12800 psi2 mm/min, @ 5% strain; ISO 178
Flexural Modulus 3.00 GPa435 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO) 160 kJ/m²76.1 ft-lb/in²ISO 180-1U
Charpy Impact Unnotched 16.0 J/cm²76.1 ft-lb/in²ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant  3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
IEC 60250
 3.6
@Frequency 100 Hz
3.6
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0077
@Frequency 100 Hz
0.0077
@Frequency 100 Hz
IEC 60250
 0.0148
@Frequency 1e+6 Hz
0.0148
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2; Parallel to Flow
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 132 °C270 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C198 °FISO 75-1,-2
Vicat Softening Point  160 °C
@Load 5.10 kg
320 °F
@Load 11.2 lb
50°C/hour; ISO 306
 245 °C
@Load 1.02 kg
473 °F
@Load 2.25 lb
120°C/hour; ISO 306
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °FInjection Molding; ISO 294
Mold Temperature 80.0 °C176 °FInjection Molding; ISO 294
Injection Velocity 40.0 mm/sec1.57 in/secInjection Molding; ISO 294

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 1310-11 NF2001 PA66 (Dry)
Celanese CoolPoly® D3612 Thermally Conductive Polyamide (PA66/6)
BASF Ultramid® 1000-11 NF2001 PA66 (Dry)
Asahi Kasei Thermylon® N3-25FG-2726 PA66-GF25
Envalior Akulon® S223-D PA66, Dry

PINEA911 / 107182

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.