MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Mobility and Materials Betaseal™ 15830E Polyurethane Adhesive
Categories: Polymer; Adhesive; Thermoplastic; Polyurethane, TP

Material Notes: One component, solvent free, moisture curing adhesive with excellent sag and bead stability based on polyurethane chemistry.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 - 1.24 g/cc0.0419 - 0.0448 lb/in³ISO 845
Solids Content >= 99 %>= 99 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 60 - 8060 - 80DIN 53505
Tensile Strength at Break 6.00 MPa870 psiISO 1798
Elongation at Break 150 %150 %ISO 1798
Shear Modulus 0.00300 - 0.00400 GPa0.435 - 0.580 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 ohm-cm1.00e+7 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air <= 100 °C<= 212 °FTemperature stability
Minimum Service Temperature, Air -40.0 °C-40.0 °FTemperature stability
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 40.0 °C50.0 - 104 °F
Shelf Life 6.00 Month
@Temperature 5.00 - 25.0 °C
6.00 Month
@Temperature 41.0 - 77.0 °F
in unopened containers. Short term storage temperatures: 0°C to +40°C.
 
Descriptive Properties
BasisPolyurethane prepolymers
ColorBlack
CompatibilityGlass
Extrusion Viscosity6 to 1423°C, 2mm / 4bar
PolymerAdhesive
Regional AvailabilityEurope
 Near East/Africa
Sagging< 30°On vertical wall
Skinning time15 - 35 Minutes.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDTF9143 / 254236

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.