MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Poco Graphite Premium Graphite Glass Forming Graphite GF-LT Graphite
Categories: Carbon; Graphite

Material Notes: GLASSMATE® materials are produced using a proprietary process that enhances material properties, surpassing that of traditional graphites. The properties of these grades have been developed to optimally match the smart glass the molds are being used for. GF-LT graphite offers the same attributes as GLASSMATE® GF plus improved wear and erosion resistance. The higher hardness of this material provides superior polishing capabilities to a very high-gloss surface finish. Features: World class microstructure. Higher level of interconnected porosity. Tighter correlation between particle and pore. Improved purity levels. Isotropic mechanical properties. Increased machining capabilities. Higher physical strength.

Information provided by Entegris POCO Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.77 g/cc
Particle Size <= 3.0 µm
Pore Size 0.800 microns
Ash <= 0.30 %< 3000 ppm ash
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 96
Flexural Strength 14150 psiMeasured using three-point bend method.
Compressive Strength 22500 psi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00245 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.50 µm/m-°C
Thermal Conductivity 60.0 W/m-KRoom temperature; as temperature increases, thermal conductivity decreases.
Maximum Service Temperature, Air 470 °COxidation threshold; weight loss after 24 hours is about 1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CPOCO402 / 268787

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.