MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
3D Systems LaserForm® Ni625 (B), AS-BUILT Nickel Super Alloy
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Tool Steel

Material Notes: Ni625 fine-tuned for use with ProX® DMP 200 metal printers producing industrial parts with high heat resistance, high strength and high corrosion resistance. LaserForm Ni625 (B) is especially resistant to crevice and pitting corrosion. LaserForm Ni625 (B) is formulated and fine-tuned specifically for 3D Systems DMP 200 metal 3D Printers to deliver high part quality and consistent part properties.

Ni625 is known for its combination of high strength and excellent corrosion resistance. LaserForm Ni625 (B) is used where these two attributes need to come together: chemical, marine, aerospace and nuclear industry. Applications include: reaction vessels, tubing, heat exchangers, valves, engine exhaust systems, turbine seals, propeller blades, submarine fittings, propulsion motors, reactor core and control-rod components in nuclear water reactors.

Classification: The chemical composition of LaserForm Ni625 (B) corresponds to ASTM F3056, UNS N06625, Werkstoff Nr. 2.4856, DIN NiCr22Mo9Nb and AMS 5666.

Information provided by 3D Systems

Key Words: ASTM F3056, UNS N06625, Werkstoff Nr. 2.4856, DIN NiCr22Mo9Nb and AMS 5666
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.44 g/ccAbsolute theoretical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 27 - 33ISO 6508-1
Tensile Strength, Ultimate 960 - 1080 MPaVertical direction - Z; ASTM E8M
 1060 - 1180 MPaHorizontal direction - XY; ASTM E8M
Tensile Strength, Yield 680 - 800 MPaRp0.2%, Vertical direction - Z; ASTM E8M
 795 - 915 MPaRp0.2%, Horizontal direction - XY; ASTM E8M
Elongation at Break 22 - 34 %Horizontal direction - XY; ASTM E8M
 27 - 35 %Vertical direction - Z; ASTM E8M
Reduction of Area 27 - 35 %Vertical direction - Z; ASTM E8M
 26 - 38 %Horizontal direction - XY; ASTM E8M
Tensile Modulus 15000 - 19000 MPaYoungs, Vertical direction - Z; ASTM E8M
 20000 - 24000 MPaYoungs, Horizontal direction — XY; ASTM E8M
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
Thermal Conductivity 9.80 W/m-K
Melting Point 1290 - 1350 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.40 %
Carbon, C <= 0.10 %
Cobalt, Co <= 1.0 %
Manganese, Mn <= 0.50 %
Molybdenum, Mo 8.0 - 10 %
Nickel, Ni 59.92 - 68.85 %Balance
Niobium, Nb (Columbium, Cb) 3.15 - 4.15 %
Phosphorus, P <= 0.015 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.015 %
Titanium, Ti <= 0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAPPR3134 / 239102

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.