Gold Ink C2090415D1 is a fritted system that has been designed as a screen printing paste for firing onto high temperature substrates. This Materials is suitable for single fire applications. This product is RoHS Compliant. Screen Printing Equipment: semi-automatic, manual Screen Types: stainless steel, polyester, mesh 230-325 tpi Substrate: Alumina and other high temperature substratesInformation provided by Gwent Electronic Materials Ltd. |