MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 VersaTrans® LV ATF Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: Phillips 66® VersaTrans® LV ATF is a full-synthetic, low-viscosity (LV) transmission fluid approved for use in passenger car and light truck automatic transmissions that require a Ford MERCON® LV or GM DEXRON®-VI fluid. It also is recommended for use in Toyota vehicles where a Type WS fluid is specified, and in many newer import vehicles. VersaTrans LV ATF is specifically engineered to help ensure long service life and to provide consistent shift performance for the life of the fluid, as well as better shift performance under extreme operating conditions. It is highly shear stable and has excellent oxidation resistance for long fluid life. It provides excellent anti-shudder performance and has excellent low-temperature properties for easier shifting in cold weather. The low-viscosity fluid results in less frictional drag (churning loss) for improved transmission efficiency, thereby offering the potential for improved fuel economy performance. VersaTrans LV ATF is recommended for use in many newer Ford, GM and Japanese vehicles where the manufacturer recommends MERCON LV, DEXRONVI, AW-1, DW-1, SP-IV, Type T-IV or Type WS fluids. It is not recommended for use in dual clutch transmissions (DCTs), belt or chain-driven continuously variable transmissions (CVTs), or older transmissions that require a higher-viscosity fluid.

Applications:

  • Ford automatic transmissions and transaxles where a MERCON LV fluid is specified
  • GM automatic transmissions where a DEXRON-VI, earlier-generation DEXRON or AW-1 fluid is specified
  • Acura and Honda automatic transmissions where a Z1 or DW-1 fluid is specified
  • Hyundai, Kia and Mitsubishi automatic transmissions where a SP-III or SP-IV type fluid is specified
  • Toyota automatic transmissions where a Type T-IV (JWS 3309) or Type WS (JWS 3324) fluid is specified
  • Hybrid vehicles with electronic continuously variable transmissions (eCVTs) where the OEM specifies a MERCON LV or Toyota Type WS fluid
  • Hydraulic systems on industrial and mobile equipment operating over a wide temperature range
VersaTrans LV ATF is OEM-approved for service fill in applications where the OEM specifies:
  • Ford MERCON® LV (License Nos. MLV140201, MLV140202, MLV140203)
  • GM DEXRON®-VI (License No. J-60175)
Features/Benefits:
  • Outstanding friction durability for consistent shift performance for the life of the fluid
  • Excellent oxidation resistance and thermal stability for long fluid life
  • Protects against sludge and varnish formation
  • Protects against rust, corrosion and wear
  • High shear stability
  • Excellent low-temperature properties for easier shifting in cold weather
  • Good seal compatibility
  • Good foam resistance
  • Low viscosity for improved fuel economy performance

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.845 g/cc
Density 7.03 lb/gal
Brookfield Viscosity 10200 cP
@Temperature -40.0 °C
Viscosity Measurement 152Index
Kinematic Viscosity at 40°C (104°F) 29.2 cSt
Kinematic Viscosity at 100°C (212°F) 5.9 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point <= -40.0 °C
Flash Point 220 °C
 
Component Elements PropertiesOriginal ValueComments
Zinc, Zn <= 0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5452 / 198705

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.