Data provided by DuPont Packaging Polymers. A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior package characteristics, and a tough, durable wrap are required. Excellent shrinkage and seal strength are obtained under a wide range of operating conditions. |