MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin HNA033 Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ HNA033 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade is heat stabilized and impact modified and was designed to withstand high heat autoclave sterilization <350 cycles. In addition, this grade is US FDA and European Food Contact approved, biocompatible (ISO10993 or USP Class VI), RoHS compliant, and it is subject to SABIC’s Healthcare management of change and formulation lock. NORYL HNA033 resin may be an excellent candidate for applications requiring multiple sterilization cycles such as disposable dental xray mouth guards and surgical stapler components.

Features: Hydrolytic Stability,Low Creep Sensitivity,Steam Sterilizable,Radiation Sterilizable,Gamma Sterilizable,Ethylene Oxide Sterilizable,E-beam Sterilizable,Low Warpage,Food Contact Acceptable,Biocompatible

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Density 1.08 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.0500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.15 %ISO 62-1
Viscosity 8.0 cP
@Load 5.00 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 8.3 g/10 min
@Load 5.00 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 55.0 MPa50 mm/min; ISO 527
 57.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 68.0 MPa50 mm/min; ISO 527
 71.0 MPa50 mm/min; ASTM D638
Elongation at Break 14.8 %50 mm/min; ISO 527
 30 %50 mm/min; ASTM D638
Elongation at Yield 5.2 %50 mm/min; ISO 527
 5.3 %50 mm/min; ASTM D638
Tensile Modulus 2310 MPa5 mm/min; ASTM D638
 2600 MPa1 mm/min; ISO 527
Flexural Strength 100 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 107 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2460 MPa1.3 mm/min, 50 mm span; ASTM D790
 2590 MPa2 mm/min; ISO 178
Izod Impact Notched 192 JASTM D256
 144 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 16.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 15.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 47.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 70.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 68.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 68.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 141 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 140 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 160 °CRate B/50; ISO 306
 161 °CRate B/50; ASTM D1525
 162 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 310 °C
Zone 2 260 - 305 °C
Zone 3 270 - 310 °C
Melt Temperature 280 - 310 °CInjection Molding
Mold Temperature 75.0 - 105 °C
Drying Temperature 105 - 110 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82336 / 290283

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.