Celanese SO.F.TER Norfor® 130 GF/30 V0 PPE compound
Categories:
Polymer
;
Thermoplastic
;
Polyphenylene Ether/PPO
;
Polyphenylene Ether, 30% Glass Filled
Material Notes:
Flame Retardant PPE compound, 30% Glass fiber, high stiffness, good dimensional stability and thermal resistance
Information provided by SO.F.TER. Spa
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.35
g/cc
0.0488
lb/in³
ASTM D1505
Linear Mold Shrinkage
0.0010
-
0.0030
cm/cm
0.0010
-
0.0030
in/in
ASTM D955
Melt Flow
8.0
g/10 min
8.0
g/10 min
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
85.0
MPa
12300
psi
ASTM D638
Elongation at Break
2.0 %
2.0 %
ASTM D638
Flexural Modulus
6.00
GPa
870
ksi
ASTM D790
Izod Impact, Notched
0.900
J/cm
1.69
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Vicat Softening Point
132
°C
270
°F
120°C/h at 50 N; ASTM D1525
Flammability, UL94
V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Glow Wire Flammability Index
960
°C
1760
°F
IEC 695-2-12
Processing Properties
Metric
English
Comments
Processing Temperature
270
-
280
°C
518
-
536
°F
Cylinder Temperature
Mold Temperature
100
-
120
°C
212
-
248
°F
Drying Temperature
80.0
°C
@Time 7200 sec
176
°F
@Time 2.00 hour
Descriptive Properties
Needle Flame Test
Passes
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Cossa Polimeri ESTAPROP 0540 GFC V0 Flame Retardant Polypropylene, 20% Glass Filled
EMS-Grivory Grilon® TSG-30/4 V0 PA666-GF30 FR
Cossa Polimeri ESTAPROP 1540 GFC V0 H Flame Retardant Polypropylene, 20% Glass Filled
PSOFS968 / 162432
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.