MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Silicones SCS1000 One-component Acetoxy Silicone Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: SCS1000 Contractors silicone sealant is a one-component acetoxy silicone material that provides excellent weatherability and elasticity for general purpose sealing and bonding. SCS1000 silicone sealant is a paste material, which cures into a flexible rubber when exposed to atmospheric moisture.

Features: Silicone Durability, ±25% Movement Capacity, Thermal Stability, Low VOC. Application: Fast Cure Time, Durable Adhesion, Gunnability, Workability. SCS1000 sealant is a candidate for use: In general purpose sealing & glazing applications. As a formed-in-place rubber gasket seal on a variety of materials and for sealing of: sheet metal, skylights, HVAC component, glass block, metal/plastic signs, marine hardware. For bedding and grouting of bathroom and kitchen tiles. As a seal around bathroom fixtures and countertops, air dryers and drains. For increased mold and mildew resistance, consider SCS1700 Sanitary.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content 20 g/lUncured; WPSTM C1454
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 27ASTM D2240
Tensile Strength, Ultimate 2.10 MPaASTM D412
Elongation, Ultimate 433 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air -55.0 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 23.0 °C
@Time 1.81e+6 sec
Cure as Tested at 50% RH
Cure Time 24.0 hour1/4" deep section, 50% RH.
Tack-Free Time 15.0 - 30.0 min
@Temperature 22.8 °C
50% RH; ASTM C679
Working Life 5.00 - 10.0 min
 
Descriptive Properties
AppearancePaste
ColorAluminum / metallicSCS1009
 BlackSCS1003
 BronzeSCS1097
 TranslucentSCS1001
 WhiteSCS1002
Silicone Content (%)100Uncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9926 / 265737

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.