MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Parson Adhesives SONLOCK™ 3567 Anaerobic Thread Sealant with PTFE
Categories: Polymer; Adhesive; Thermoset

Material Notes: SONLOK 3567 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The high lubricating properties of this compound prevent galling on stainless steel, aluminum and all other metal pipe threads and fittings. UL Classification: Classified as small fire hazard. No flash point in liquid state. Ignition temperature 465°C. For use in devices handling gasoline, petroleum oils, natural gas, propane and butane.

Applications:

  • Recommended for industrial applications in the chemical processing, petroleum refining, pulp/paper, waste treatment, textile, utilities/power generation, marine, automotive, industrial equipment, gas compression and distribution industries.
  • Widely used for industrial plant fluid power systems.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/cc
Brookfield Viscosity 540000 cPRVT, Spindle 3 @ 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 147 psiSteel Pins & Collars; ISO 10123
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696 K-1
Specific Heat Capacity 0.300 J/g-°C
Thermal Conductivity 0.100 W/m-KASTM C177
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -65.0 °F
Flash Point >= 100 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 4.00 hourFunctional
 10.0 - 30.0 minHandling
 24.0 hourFull
 
Descriptive Properties
ColorWhite
CompositionMethacrylate Ester
Initial Strength Retained (%)100Motor Oil for 500 hrs at 125°C
 100Motor Oil for 1000 hrs at 125°C
 100Break Fluid for 500 hrs at 22°C
 60Acetone for 1000 hrs at 22°C
 70Acetone for 500 hrs at 22°C
 75Water/Glycol for 500 hrs at 87°C
 75Water/Glycol for 1000 hrs at 87°C
 80Gasoline for 500 hrs at 22°C
 80Gasoline for 1000 hrs at 22°C
 90Ethanol for 500 hrs at 22°C
 90Ethanol for 1000 hrs at 22°C
 95Break Fluid for 1000 hrs at 22°C
Solvent ContentNone
Torque>1.75 NmBreakaway, M10 steel nuts and bolts, ISO 10964
 1 NmPrevail, M10 steel nuts and bolts, ISO 10964

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPARSN041 / 186484

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.