MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Resin Technology Group TIGA 202-EX High Performance, Fast Cure Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Mix ratio 2 to 1 by volume.

TIGA 202-EX is a two-part epoxy adhesive offering outstanding shear tensile and peel adhesion. TIGA 202-EX offers a 20 minute pot life and good hardness development within 1 hour of mixing. TIGA 202-EX is a toughened epoxy exhibiting rugged chemical and environmental resistance and durability. TIGA 202-EX is an excellent general purpose adhesive providing exceptional bond strength to a wide variety of substrates, PVC, FRP, Polyacrylic, Steel, and many more.

Applications:

TIGA 202-EX is excellent for general purpose high speed industrial assembly, electronic applications, component attachment to boards, housing assembly and potting.

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccOf resin
 1.13 g/cc1.13 g/ccOf hardener
Viscosity 60000 cP
@Temperature 25.0 °C
60000 cP
@Temperature 77.0 °F
Mixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 45 - 5545 - 55Cured 2 hours at 25°C
 75 - 8575 - 85Cured 24 hours at 25°C
 75 - 8575 - 85
Shear Strength >= 27.6 MPa>= 4000 psi2 hours, 65°C
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 65.0 °C
0.500 hour
@Temperature 149 °F
 720 - 1200 min
@Temperature 25.0 °C
12.0 - 20.0 hour
@Temperature 77.0 °F
Pot Life 20 - 30 min20 - 30 minSmall Mass(15gr.)
 
Descriptive Properties
ColorOff-white/Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Resin Technology Group TIGA 108 Room Temperature Curing Epoxy Adhesive
Resin Technology Group KONA 877 Low Viscosity, Low Shrinkage, Vacuum Grade Casting Resin
Resin Technology Group TIGA HTR-815 High Temperature Resistant, Rigid Thermally Conductive Epoxy
Resin Technology Group TIGA F-715 Rome Temperature Curing, Rigid Thermally Conductive Epoxy
Resin Technology Group KONA 871 Low Cost Epoxy Resin

PRESINT632 / 65516

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.