MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Oceanchem Group ANTIOXIDANT SK-225
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Cas No.: 6683-19-8

Properties: Antioxidant SK-225 is a kind of compound components, including antioxidant SK-1010 and antioxidant SK-168. Soluble in benzene, hexane, ethyl acetate, insoluble in water.

Uses: Antioxidant SK-225, with good synergistic of antioxidant SK-1010 and SK-168, can retard heated degradation and oxidative degradation of polymeric substances during processing and in end applications. It can be widely used for PE, PP, PC, ABS resin and other petro-products. The amount to be used may be 0.1-0.8%.

Package and Storage: Packed with plastic bag in composite plastic woven sack, net 25 kg/bag. Store in a cool area designed for the storage of chemicals. Period of Validity: Normally 6 months.

Information Provided by Oceanchem Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  >= 96 %
@Wavelength 425 nm
>= 96 %
@Wavelength 425 nm
 >= 97 %
@Wavelength 500 nm
>= 97 %
@Wavelength 500 nm
 
Descriptive Properties
AppearanceClear white powder
CAS Number6683-19-8
Content of Antioxidant45.0-55.0Antioxidant SK-168
 45.0-55.0Antioxidant SK-1010

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POCEAN55 / 104259

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.