MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC SABIC® PP 7705 PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PPcompound 7705 is a mineral filled modified polypropylene. This material combines high scratch resistance, high stiffness, good impact and high flow. This material has a very broad processing window combined with good esthetical performance. Typical applications include esthetical automotive interior parts such as instrument panels, lower and upper dashboard, door panels and trim. SABIC® PPcompound 7705 is a designated automotive grade. IMDS ID: 16161010

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³Injection molded sample ISO527-1A; ISO 1183
Linear Mold Shrinkage 0.0085 cm/cm0.0085 in/inInjection molded plaque 65x65x3.2mm; SABIC method
Melt Flow 22 g/10 min
@Load 2.16 kg,
Temperature 230 °C
22 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 17.0 MPa2470 psiISO 527/1A
Tensile Strength, Yield 22.0 MPa3190 psiISO 527/1A
Elongation at Break 35 %35 %ISO 527/1A
Tensile Modulus 1.80 GPa261 ksiISO 527/1A
Flexural Modulus 1.90 GPa276 ksiISO 178/1A
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²N.B.: No Break; ISO 180/1A
 4.00 kJ/m²
@Temperature -20.0 °C
1.90 ft-lb/in²
@Temperature -4.00 °F
N.B.: No Break; ISO 180/1A
 6.00 kJ/m²
@Temperature 0.000 °C
2.86 ft-lb/in²
@Temperature 32.0 °F
N.B.: No Break; ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 73.0 µm/m-°C
@Temperature -30.0 - 100 °C
40.6 µin/in-°F
@Temperature -22.0 - 212 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °FISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11316 / 244783

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.