MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CTC X-PRO TF 1120 HP Polypropylene Homopolymer, 20% Talc Filled  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: X-PRO TF 1120 HP is a 20% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, fan and lighting shrouds, HVAC components, lawn & garden, pipe fittings, and appliances.

Data provided by Composite Technologies (CTC).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 20 g/10 minISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 31.0 MPaISO 527-1/2
Flexural Modulus 2500 MPa0.05 in/min; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²Low Temp; ISO 180/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 245 °FASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 150 °FASTM-D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 400 - 420 °F
Middle Barrel Temperature 420 - 440 °F
Front Barrel Temperature 440 - 460 °F
Melt Temperature 440 - 460 °F
Mold Temperature 80.0 - 140 °F
Back Pressure 100 - 150 psi
Clamp Pressure 4000 - 5000 psi
 
Descriptive Properties
Boost Pressure (psi)750-1500
Hold Pressure50 - 75% of Boost
Screw SpeedFast

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene Homopolymer HP0339T20L1 Talc Reinforced
LyondellBasell Hostacom EYC 136N T 1064 (MARBLE) Polypropylene Copolymer, 13% Talc Filled
Mytex Polymers AS33K(W)-02 Polypropylene, Talc filled, Compounded
LyondellBasell Hostacom X M2 V05/M T 3130 Polypropylene with 20% Talc Filler
RheTech Products HP514-00UV 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural

PCTC956 / 104729

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.