MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chisso Z CLEAN® E1001 Purging Solution
Categories: Polymer; Thermoplastic; Purging Compound

Material Notes: Z Clean Grade E1001 is recommended for hot runner systems and extrusions.

General Z Clean information: Z CLEAN has high cleaning power - effective at penetrating and swelling to clean the inside of nozzles and dies - and eliminates black specking. It comes in easy to handle pellets. Z CLEAN can be used in the range 160-400°C. It is non-abrasive and non-toxic. Z CLEAN comes in several grades to work with almost any thermoplastic - PP, PE, PS, ABS, PVC, PA, PC, PPO, PEEK, PPS, LCP, etc. It can be used in a variety of molding equipment - injection, extrusion, and blow molding. Z CLEAN has high heat stability and generates no odor or smoke.

Manufactured by Chisso Corporation.

Key Words: Chisso Corporation; purge; Zclean; Z-clean
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chisso Z CLEAN® A1 Purging Solution
Chisso Z CLEAN® S29 Purging Solution

PX0006 / 72834

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.