HumiSeal® UV50LV is a one-part, low viscosity, high solids dual cure acrylated polyurethane conformal coating possessing excellent chemical resistance, flexibility and moisture resistance. HumiSeal® UV50LV has been developed at a low viscosity to allow use with film coater type selective coating equipment. HumiSeal® UV50LV is tack free after exposure to UV light and the secondary moisture cure mechanism will fully cure any unexposed areas of the coating within 7 days at ambient conditions. Cured HumiSeal® UV50LV has a higher flexibility compared to other UV curable conformal coatings, giving improved performance in thermal cycling tests. HumiSeal® UV50LV fluoresces under UV light to allow coating inspection and can be applied by all selective coating equipment. HumiSeal® UV50LV contains no VOCs or solvent. HumiSeal® UV50LV is recognized under UL File Number E105698.Information provided by Chase Electronic Coatings. |