MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Lucas-Milhaupt SIL-FOS® 6 Silver/ Copper/ Phosphorus Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes:

Applications: Sil-Fos 6 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in service. It should only be used on assemblies where good fitup can be maintained.

Characteristics:Sil-Fos 6 is a copper-rich, intermediate temperature, brazing filler metal that is free-flowing and self-fluxing on copper by virtue of its phosphorus content. This alloy is extremely fluid when heated rapidly to its flow point and will penetrate joints with very little clearance. Best results are obtained with joint clearances of .001-.003 in.

Sil-Fos 6 liquates (i.e. separates into high and low melting constituents) if heated slowly through its melting range.

The self-fluxing property of Sil-Fos 6 is effective on copper only. Copper base alloys, such as brass or bronze, may be brazed with Sil-Fos 6 if the joints are coated with Handy Flux. Sil-Fos 6 should not be used on ferrous metals or nickel base alloys, since the phosphorus produces brittle iron or nickel phosphorus at the joint interface.

Specifications:This alloy conforms to the following specifications: AWS A5.8 BCuP-4, ASME Boiler & Pressure Vessel Code, Sec.II-C, SFA5.8 BCuP-4

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.86 g/cc0.284 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000219 ohm-cm0.0000219 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 640.6 - 718.3 °C1185 - 1325 °F
Solidus 640.6 °C1185 °FMelting Point
Liquidus 718.3 °C1325 °FFlow Point
 
Processing PropertiesMetricEnglishComments
Processing Temperature 690.6 - 788 °C1275 - 1450 °FBrazing Range
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 86.15 %>= 86.15 %
Other, total <= 0.15 %<= 0.15 %
Phosphorus, P 7.0 - 7.5 %7.0 - 7.5 %
Silver, Ag 5.8 - 6.2 %5.8 - 6.2 %
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NLUCMI51 / 18118

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.