MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Hexamethylenediamine 70%
Categories: Fluid

Material Notes: Recommended use: For the production of homopolymerisates and copolymerisates, initial product for chemical syntheses

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc
@Temperature 40.0 °C
0.0332 lb/in³
@Temperature 104 °F
pH 12.412.4100 g/l
Viscosity 0.90 cP
@Temperature 40.0 °C
0.90 cP
@Temperature 104 °F
Dynamic
Vapor Pressure 0.0400 bar
@Temperature 50.0 °C
30.0 torr
@Temperature 122 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 5.50 °C41.9 °FSolidification
Boiling Point 111.5 °C232.7 °F
Flash Point >= 85.0 °C>= 185 °FDirective 92/69/EEC, A.9
Ignition Temperature 305 °C581 °FDIN 51794
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Hexamethylenediamine
Syensqo (Solvay Specialty Polymers) Rhodiamine™ Hexamethylene diamine
Radici Radilon® A 35E 990 (dry) Nylon 66
BASF N3-Amine 3-(2-aminoethylamino)propylamine

PBASG0216 / 131849

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.