MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay Toolcoat S/T-05 S/A Adhesive tape
Categories: Polymer; Adhesive; Tape

Material Notes: Description: Adhesive tape. Ideally suited for tool surface release applications.

Features & Benefits:

  • Skived TFE tape, with a high temperature pressure sensitive, fully cured silicone adhesive (Toolcoat S/T A)
  • Can be used on several contoured bond jigs and lay-up molds, due to its high conformability
  • Its properties make it inert to almost all chemicals, corrosives and environmental factors.
  • Eliminates the need for liquid or paste release coatings on tool surface and is especially useful on composite tools and press platens.
  • While Toolcoat S/T gives optimum release, other applications are flash control, heat-sealing machines, covering of coating and drying rolls, chute lining, lining for guide rails, and any other non-stick, low fiction applications.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 130 micronsAdhesive
 170 micronsTotal
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 275 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 288 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCYTED238 / 180540

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.