MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Lanxess Addovate® Thermostab Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Addovate Thermostab belongs to the material group of organic phosphite and is used as non-ionic, sterically hindered antioxidant acting against thermo-oxidative degradation which may occur during processing as a result of thermal, oxidative and mechanical stress.

Use: The main fields of application of Addovate Thermostab are the stabilization of PC/ABS, PA/ABS, TPU, ABS and PA against thermo-oxidative degradation during processing in the melt.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.620 g/cc0.0224 lb/in³powder
 0.700 g/cc0.0253 lb/in³pastilles
 
Chemical PropertiesMetricEnglishComments
Acid Value 1010[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Melting Point 182 - 185 °C360 - 365 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AppearancePellets or powder
Coloryellowish

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8231 / 208624

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.