System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC LEXAN™ VISUALFX™ Resin FXD123R Polycarbonate (PC) (Asia)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
LEXAN FXD123R is a transparent/translucent low viscosity grade for light diffusion special effects. UV-stabilized. Color package may affect performance.
Features: UV Resistant,Aesthetics & Visual effects
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.20
g/cc
1.20
g/cc
ASTM D792
Water Absorption
0.15 %
@Time 86400 sec
0.15 %
@Time 24.0 hour
ASTM D570
Moisture Absorption
0.0200 %
0.0200 %
Injection Molding
Linear Mold Shrinkage, Flow
0.0050
-
0.0070
cm/cm
@Thickness 3.20 mm
0.0050
-
0.0070
in/in
@Thickness 0.126 in
SABIC method
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
123
123
ASTM D785
Tensile Strength, Yield
61.0
MPa
8850
psi
SABIC - Japan Method
Elongation at Break
220 %
220 %
SABIC - Japan Method
Flexural Strength
93.0
MPa
13500
psi
ASTM D790
Flexural Modulus
2.20
GPa
319
ksi
ASTM D790
Izod Impact Notched
735
J
542
ft-lb
ASTM D256
Electrical Properties
Metric
English
Comments
Surface Resistance
1.00e+16
ohm
1.00e+16
ohm
ASTM D257
Dielectric Constant
3.2
@Frequency 50.0 - 60.0 Hz
3.2
@Frequency 50.0 - 60.0 Hz
ASTM D150
Comparative Tracking Index
250
-
400
V
250
-
400
V
UL 746A
Hot Wire Ignition, HWI
7.0
-
15
sec
@Thickness >=1.50 mm
7.0
-
15
sec
@Thickness >=0.0591 in
UL 746A
High Amp Arc Ignition, HAI
30
-
60
arcs
@Thickness >=1.50 mm
30
-
60
arcs
@Thickness >=0.0591 in
UL 746A
60
-
120
arcs
@Thickness >=3.00 mm
60
-
120
arcs
@Thickness >=0.118 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR
25.4
-
80.0
mm/min
1.00
-
3.15
in/min
UL 746A
Thermal Properties
Metric
English
Comments
CTE, linear
70.0
µm/m-°C
@Temperature -30.0 - 30.0 °C
38.9
µin/in-°F
@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi)
130
°C
@Thickness 3.20 mm
266
°F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical
130
°C
266
°F
UL 746B
UL RTI, Mechanical with Impact
130
°C
266
°F
UL 746B
UL RTI, Mechanical without Impact
130
°C
266
°F
UL 746B
Flammability, UL94
HB
@Thickness >=0.750 mm
HB
@Thickness >=0.0295 in
UL 94
Processing Properties
Metric
English
Comments
Nozzle Temperature
270
-
290
°C
518
-
554
°F
Zone 2
270
-
290
°C
518
-
554
°F
Zone 3
280
-
300
°C
536
-
572
°F
Melt Temperature
280
-
300
°C
536
-
572
°F
Injection Molding
Mold Temperature
80.0
-
100
°C
176
-
212
°F
Drying Temperature
120
°C
248
°F
Injection Molding
Dry Time
2.00
-
4.00
hour
2.00
-
4.00
hour
Injection Molding
Precipitation Temperature
60.0
-
80.0
°C
140
-
176
°F
Hopper Temperature
Descriptive Properties
UV-light, water exposure/immersion
F1
UL 746C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH80504 / 288451
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.