MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SunChemical Gwent C2041206P2 Gold Polymer Electrode Paste
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Gold paste is a screen printable gold polymer paste designed as a working electrode in electrochemical biosensors. This is used as a working electrode in medical diagnostics, environmental sensor and the ’agri-food’ industries, in conjunction with our counter electrodes and reference electrodes. The paste is suitable for self-assembled monolayers, DNA and immuno-sensors.
Screen Printing Equipment: semi-automatic, manual
Screen Types: stainless steel, polyester, mesh 230-325tpi
Substrate: polyester, PVC, polycarbonate and alumina

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 80 - 82 %
@Temperature 700 °C
80 - 82 %
@Temperature 1290 °F
Viscosity 12000 - 18000 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
12000 - 18000 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 27.0 microns1.06 milPrinted through a 230ss mesh
Storage Temperature 20.0 °C68.0 °Fsealed container
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 110 ohm
@Thickness 0.0270 mm
110 ohm
@Thickness 0.00106 in
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 180 °C
0.500 hour
@Temperature 356 °F
 60.0 min
@Temperature 60.0 °C
1.00 hour
@Temperature 140 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Coverage cm2/g90Using a 230 mesh stainless steel screen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SunChemical Gwent C2041206D2 Gold Polymer Electrode Paste

WGELZ9015 / 139328

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.