MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik TEGOPREN® 6846 Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product description: TEGOPREN® 6846 is an organic modified siloxane based wax, especially designed to improve the processing and final performance of polyolefin.

Application: TEGOPREN® 6846 is used as a semi-compatible slip and release agent for various end uses.

Benefits: During the extrusion process TEGOPREN® 6846 improves the flow characteristics. This results in:

  • reduction of shear during the extrusion of polyolefin with low MFI
  • reduction of amperage values, which means lower energy consumption
  • higher throughput during the extrusion
  • improved cycle time/less machine down time
TEGOPREN® 6846 combines the properties of the organic modification and the typical characteristics of a siloxane. This results in improved characteristics of the polymer:
  • smooth processing during down-stream application, especially during foam extrusion
  • no negative impact on printability/sealability smoother surface of films can be easily deter-mined by lower COF values
  • improved slip properties

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 70 cP70 cP
 
Thermal PropertiesMetricEnglishComments
Melting Point 64.0 °C147 °F
Flash Point 250 °C482 °Fmelt
 
Descriptive Properties
Appearancepellet
Content45%Active matter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TEGOPREN® 5847 Additive
Evonik TEGOPREN® 5852 Additive
Evonik TEGOPREN® 5885 Additive
Evonik TEGO® Antifoam 2290 Antifoam concentrate
Evonik TEGOPREN® 5851 Defoamer

PEVONIL605 / 196809

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.