MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Chemlon® A60XT Nylon 66, Impact Modified
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Notes: A60XT is a modified nylon 66 that offers high impact strength coupled with good rigidity.

Availability: Europe

Additive: Impact Modifier

Features: High Impact Resistance; Impact Modified; Medium Rigidity

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.3 %2.3 %50% RH; ISO 62
Linear Mold Shrinkage 0.016 - 0.023 cm/cm0.016 - 0.023 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 58.0 MPa8410 psiISO 527-2
Elongation at Break 30 %30 %ISO 527-2
Elongation at Yield 6.0 %6.0 %ISO 527-2
Tensile Modulus 2.10 GPa305 ksiISO 527-2
Flexural Strength 65.0 MPa9430 psiISO 178
Flexural Modulus 2.00 GPa290 ksiISO 178
Charpy Impact, Notched 3.57 J/cm²17.0 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 185 °C365 °FUnannealed; ISO 72-2/B
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FUnannealed; ISO 72-2/A
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
Oxygen Index 22 %22 %ISO 4589-2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 - 290 °C518 - 554 °F
Middle Barrel Temperature 270 - 290 °C518 - 554 °F
Front Barrel Temperature 270 - 290 °C518 - 554 °F
Melt Temperature 270 - 290 °C518 - 554 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sax Polymers SAXAMID 236Q33 Nylon 6.6, Impact Modified
CP-Polymer-Technik Wellamid® 6600/58 HWCP Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry
CP-Polymer-Technik Wellamid® 6600/58 HWCP Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Conditioned
CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Dry
CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Conditioned

PTEKNQ0544 / 237035

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.