MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil Santoprene® 8291-65TB Thermoplastic Rubber  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: A colorable thermoplastic elastomer which bonds to adhesive/epoxy spin-finished polyester or standard nylon fibers for closed-braid hose and woven-substrate products. With bonds stronger than the TPE itself, it generates new applications for TPE's including industrial hose, lightweight conveyor belting and fabric reinforced sheet. It can be processed using co-extrusion or other melt processing techniques. Supplied as free-flowing pellets in 25 kilogram (55 pound) moisture barrier bags.

Product Notes: Values are for injection molded plaques, side gated.
82.6 mm x 117.5 mm x 3 mm

Information provided by Advanced Elastomer Systems.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 655 seconds; ASTM D2240
Tensile Strength at Break 1000 psiAcross flow; ASTM D412
Tensile Stress at Strain 300 psi
@Strain 100 %
across flow; ASTM D412
Elongation at Break 500 %Across flow; ASTM D412
Compression Set 22 %
@Temperature 22.8 °C,
Time 612000 sec
Method B; ASTM D395
Tensile Set 11 %ASTM D412
 
Processing PropertiesOriginal ValueComments
Melt Temperature 215 - 250 °C
Drying Temperature 70.0 °CDesiccant Dryer
Dry Time 3 hourDesiccant Dryer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Advanced Elastomer Systems Santoprene® 8281-65 Thermoplastic Rubber
Advanced Elastomer Systems Santoprene® 8281-45W237 Thermoplastic Rubber
Advanced Elastomer Systems Santoprene® 8281-35W237 Thermoplastic Rubber
Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber
ExxonMobil Santoprene® 8291-80TB Thermoplastic Rubber

PADW171 / 22889

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.