MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mid-Mountain Materials CERMEX® PR1000-C Commercial Grade Thermal Insulation Paper
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Fibers

Material Notes: Material: Non-respirable E-glass fibers
Construction: Felted paper, organic binder

Information provided by Mid-Mountain Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.90 lb/ft³
@Thickness 3.17 mm
 7.00 lb/ft³
@Thickness 6.35 mm
 11.0 lb/ft³
@Thickness 1.59 mm
Loss On Ignition 5.0 - 7.0 %
Thickness 1587 microns
 3175 microns
 6360 microns
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0350 W/m-K
@Temperature 24.0 °C
N2; ASTM C177
 0.0450 W/m-K
@Temperature 100 °C
N2; ASTM C177
 0.0600 W/m-K
@Temperature 200 °C
N2; ASTM C177
 0.0600 W/m-K
@Temperature 200 °C
Air; ASTM C114
 0.0810 W/m-K
@Temperature 300 °C
Air; ASTM C114
 0.105 W/m-K
@Temperature 400 °C
Air; ASTM C114
Melting Point >= 1100 °CFiber Only
Maximum Service Temperature, Air 1000 °FContinuous
 1200 °FIntermittent
 
Descriptive Properties
ColorWhite
Tensile Strength (lbs/in)221/16", Cross Direction
 251/16", Machine Direction
 331/8", Machine Direction
 341/8", Cross Direction
 69.21/4", Machine Direction
 81.71/4", Cross Direction
Width (in)51Standard

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chosun Refractories 1260PAPER Paper
Chosun Refractories 1500 ACE PAPER Paper
ITW Insulation TRYMER® 1800 Polyisocyanurate Insulation
Thermal Ceramics BTU-GUE
3M 4317 Single-Coated Foam Tape

CMID66 / 141234

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.