MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Vinnolit® E 69 ST PVC for Paste Application
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Vinnolit® E 69 ST PVC for paste application. Vinnolit® E 69 ST is a very fine-particle, paste-making emulsion homopolymer, giving medium viscosity plastisols with a good shelf life. Plastisols made with Vinnolit® E 69 ST have a slightly pseudoplastic rheology. Vinnolit® E 69 ST exhibits excellent foaming characteristics in chemically blown foams. Due to its outstanding low coarse particle content and white color it is recommended for foamed wall coverings made by rotary screen printing or hot embossing. Noteworthy properties are: medium viscosity with pseudoplastic rheology, excellent foaming characteristics with good expansion ratio and a uniform, fine cell structure, even at high filler loading, very fine powder, suitable for screen printing, very good whiteness.

Information provided by Vinnolit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.30 %ISO 1269
Apparent Bulk Density 0.390 g/ccISO 60
Particle Size <= 100 µm<= 0.1% Retained on 0.1 mm Sieve; DIN EN ISO 53195
Viscosity Test 1.16 dl/gReduced Viscosity; ISO 1628-2
 
Descriptive Properties
Emulsifier ContentMedium
K-Value68ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVINNO945 / 291142

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.