AISI 8620 is a common, carburizing alloy steel used for a variety of medium-strength applications including gears, camshafts, fasteners, and chains/chain pins. Flexibility in hardening treatments allow optimization of case/core properties. Specific conditions for property data below: Double quenched and tempered: carburized at 925°C (1700°F) for 8 hrs., pot cooled, reheated to 845°C (1550°F), quenched in agitated oil, reheated to 800°C (1470°F), quenched in agitated oil, 150°C (300°F) temper. 1.8 mm case depth. Core properties. |
AFNOR 22 NCD 2, UNI 20 NiCrMo 2, JIS SNCM 21 H, JIS SNCM 21, B.S. 805 H 20 (UK), B.S. 805 M 20 (UK), MIL SPEC MIL-S-16794, SAE J404, SAE J770, DIN 1.6523, AFNOR 20 NCD 2 (France), UNS G86200, AMS 6274, AMS 6276, AMS 6277, ASTM A322, ASTM A331, ASTM A505, ASTM A513 |