MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond Supreme 10HTS Silver Filled Electrically Conductive One Part Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • NASA low outgassing approved
  • Excellent physical strengths
  • No mix, single component system
  • Serviceability from 4K to +400°F
  • Silver conductive
  • Resistance to mechanical and thermal shocks
Product Description: Master Bond Supreme 10HTS is a user friendly, one component, silver conductive epoxy system featuring a remarkable array of properties along with exceptionally simple processing. It requires no mixing, but does require oven curing at 250-300°F. First and foremost, this multifaceted epoxy is a splendid conductor of electricity. Its temperature resistance profile is truly dazzling; it is serviceable from 4K to +400°F. Supreme 10HTS has superb bond strength both in shear and peel. It bonds well to a variety of substrates, including metals, composites, glass, ceramics and many rubbers and plastics. It is formulated to withstand rigorous thermal cycling as well as thermal and mechanical shocks. It fully meets NASA low outgassing specifications. In addition to the properties mentioned above, Supreme 10HTS has good chemical resistance against water, oils, many fuels and a number of acids and bases. It retains its superb electrical conductivity even in adverse conditions. As a silver filled system, Supreme 10HTS is also a reliable thermal conductor. This highly versatile system is well suited for the most challenging applications in the aerospace, electronic, electro-optic, specialty OEM as well as many other types of high tech industries.

Product Advantages:

  • Single component system; no mixing needed prior to use; cures at 250-300°F
  • Easy application; requires minimal fixturing pressure
  • Commanding physical strength properties, including high bonding strength
  • Extraordinary temperature range of 4K to +400°F
  • Wonderful electrical conductivity properties; contains high purity silver
  • Passes NASA low outgassing test

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Viscosity >= 500000 cP>= 500000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 75>= 75
Tensile Strength >= 34.5 MPa>= 5000 psi
Tensile Modulus 3.10 GPa450 ksi
Adhesive Bond Strength >= 8.27 MPa>= 1200 psiTensile Lap, Aluminum to Aluminum
Peel Strength >= 2.63 kN/m>= 15.0 pli
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.0060 ohm-cm<= 0.0060 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 - 45.0 µm/m-°C22.2 - 25.0 µin/in-°F
Thermal Conductivity >= 1.59 W/m-K>= 11.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -167 °C-269 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  40.0 - 45.0 min
@Temperature 149 °C
0.667 - 0.750 hour
@Temperature 300 °F
 60.0 - 75.0 min
@Temperature 121 °C
1.00 - 1.25 hour
@Temperature 250 °F
Shelf Life 3.00 - 6.00 Month
@Temperature <=23.9 °C
3.00 - 6.00 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Descriptive Properties
ColorSilver gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond Supreme 42HT-2 Toughened Epoxy Resists Thermal Cycling
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy
Master Bond EP29LPSP Low Outgassing, Optically Clear Two Component Epoxy
Master Bond EP21TDCS Silver Filled Electrically Conductive Epoxy Compound

PMASTM956 / 185549

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.