MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LG Chemical Ethyl Acrylate  (discontinued **)
Categories: Fluid

Material Notes: Low Color - Refining process improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Acidity is the main quality factor that influence the reaction speed.

Application: Textiles Sizing Agent, Paint & Ink, Adhesives, Flexible Resin, Non woven Binder

CAS No. 140-8 8-5

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.919 - 0.923 g/cc0.919 - 0.923 g/ccHydrometer; ASTM D1298
Viscosity 0.869 cP0.869 cP
Vapor Pressure 0.0387 bar
@Temperature 20.0 °C
29.0 torr
@Temperature 68.0 °F
Vapor density: 4.4
 
Thermal PropertiesMetricEnglishComments
Melting Point -75.0 °C-103 °FFreezing Point
Boiling Point 99.6 °C211 °F
Flash Point 9.00 °C48.2 °FCC
 29.4 °C84.9 °FCC
Ignition Temperature 385 °C725 °FAutoignition
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %Karl-fischermeter; ASTM D1364
 
Descriptive Properties
Acidity<0.005
Color<10 APHAASTM D1209
Flammable limits in air1.8-12.1% (LEL)
Inhibitor (MEHQ)10-20 ppmUVSpectro, ASTM D3125
Purity>99.5%Gas Chro.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLAY353 / 148363

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.