WESTLAKE Hifor Clear Polyethylene SC74557 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and low antiblock. Films produced with this resin exhibit good toughness, with excellent gloss and clarity for a product of this density. SC74557 is well suited for packaging frozen goods, fruits and vegetables, and baked goods.Application/Uses- Frozen food films
- High clarity bread bags
- Ice bags
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical |
Good toughness, with excellent gloss and clarity |