MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese Ateva® 1075A Ethylene Vinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Ateva® 1075A resin is designed for compound and masterbatch applications, it is also suitable for extrusion and injection molding applications. This EVA resin may be safely used as articles or components of articles intended for uses in contact with food as provided in FDA regulation 21 CFR 177.1350 - Ethylene-vinyl acetate copolymers, subject to extraction limitations on the finished food-contact article as specified in that regulation. This polymer may be processed on conventional extrusion equipment. It is recommended that the melt temperature be kept below 210°C as decomposition can occur at higher temperatures. Additives: Antioxidant

Applications: Compounds & Masterbatches; Molding & Miscellaneous

Information provided by Celanese Corporation.

Key Words: designed for compound and masterbatch applications
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D1505; ASTM D1928 Proc A
Vinyl Acetate Content 9.0 %9.0 %AT Plastics PTM-39
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9494ASTM D2240
Hardness, Shore D 4646ASTM D2240
Tensile Strength at Break 15.0 MPa2180 psiType IV (50 mm/min); ASTM D638
Elongation at Break 692 %692 %Type IV (50 mm/min); ASTM D638
Flexural Modulus, 1% Secant 115 MPa16700 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 98.0 °C208 °FDSC; ASTM D3417
Vicat Softening Point 79.0 °C174 °FASTM D1525
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Ateva® 2861A Ethylene Vinyl Acetate Copolymer
Celanese Ateva® 4030AC Ethylene Vinyl Acetate Copolymer
Celanese Ateva® 1608 EVA polymer for compounds, molding and tubing
Celanese Ateva® 2606A EVA polymer for adhesives, automotive, compounds and molding
Albis Plastics Tedur® L V 9400-1 PPS, 15% Carbon Fiber

PATEVB64 / 26020

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.