MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SCG Chemicals LP1100P Refined polyethylene homopolymer wax
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: SCG PE WAX LP1100P is a refined polyethylene homopolymer wax derived from the unique HDPE process by Thai Polyethylene Co., Ltd., a subsidiary of Chemicals Business, SCG. Under the operational excellent along with the high technology (close loop refinery), LP1100P is guaranteed its high quality for various applications.

Applications: Hot melt adhesive, PVC compound, color master batch, thermoplastic road marking, plastic additive, petroleum wax blend, rubber, cable filling compound, candle.

Features: High melting and softening point. Low viscosity. Excellent heat resistance and thermal stability. High hardness level. Excellent chemical resistance. Excellent compatibility with other waxes. Excellent lubrication.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D 1505
Viscosity 60 - 100 cPASTM D3236
 
Mechanical PropertiesOriginal ValueComments
Penetration 2.0d.mm; ASTM D1321
 
Thermal PropertiesOriginal ValueComments
Dropping Point 116 °CASTM D3954
 
Descriptive Properties
AppearanceWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCGC754 / 278011

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.