HM5000 is a high density polyethylene for extrusion monofilament. HM5000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a Applications: Advantages: - Excellent processability
- High stiffness
- High draw down capability
Information provided by Titan Chemicals |