MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Kendall® Classic ATF Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: Kendall® Classic ATF is a high-quality transmission fluid recommended for use in all domestic and import vehicles no longer under warranty where the OEM previously specified a GM DEXRON®-III H or Ford MERCON® fluid. Classic ATF is formulated to provide the proper frictional characteristics for smooth, quiet shifting in electronically controlled automatic transmissions. It has excellent oxidation resistance for long fluid life, excellent low-temperature properties for easy shifting in cold weather, protects against wear and helps minimize the formation of sludge and varnish.

Applications:

  • GM and Ford automatic transmissions in 2005 and earlier model-year vehicles that are no longer under warranty, where the OEM previously specified DEXRON® -III H, DEXRON®-II, DEXRON® or MERCON® ATF
  • Import vehicles where DEXRON®-III H (obsolete) or an earlier-generation DEXRON® fluid (obsolete) is specified
  • Allison heavy-duty off-highway automatic transmissions that require a C-4 quality fluid
  • Hydraulic systems on industrial and mobile equipment operating over a wide temperature range

    Features/Benefits:

    • Proper frictional properties for smooth shifting and excellent anti-shudder performance
    • Excellent oxidation resistance and thermal stability for long fluid life
    • Excellent low-temperature properties
    • Protects against wear
    • Minimizes sludge and varnish deposits
    • Protects against rust and corrosion
    • Good seal compatibility
    • Suitable for both automotive and industrial applications

    Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.861 g/cc
Density 7.17 lb/gal
Brookfield Viscosity 14000 cP
@Temperature -40.0 °C
Viscosity Measurement 188Index
Kinematic Viscosity at 40°C (104°F) 32.1 cSt
Kinematic Viscosity at 100°C (212°F) 7.0 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point <= -40.0 °C
Flash Point 212 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Zinc, Zn <= 0.0030 %
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phillips 66 Triton® Heavy Duty ATF Automatic Transmission Fluid
Phillips 66 CVT Fluid Full-Synthetic Transmission Fluid
ELM® SoyFluid™ Hydraulic Universal Tractor Biodegradable Tractor Hydraulic-Transmission Fluid
ConocoPhillips Hydroclear® ATF Type F Automatic Transmission Fluid
ChevronTexaco Type F Automatic Transmission Fluid

WCON5300 / 198553

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.