MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
OJSC Plastic ABS 2802-31 ABS Plastic
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Extrusion Grade

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cmunder pressure
Melt Flow 1.3 - 3.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 36.3 MPasample-shovel type II, 20±2 mm/min
Elongation at Break 30 %paddle type II, 20±2mm.
Izod Impact, Notched (ISO) >= 34.3 kJ/m²sample type 1, with cut 3.2mm
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point >= 95.0 °Cload 50N; 120°C/hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Stratasys® ABS-M30
Sibur ABS 2020-60 Molding Grade ABS Plastic
Sibur ABS 1106M Extrusion Grade ABS Plastic
Proto3000 ABS-M30 Fused Deposition Modeling Polymer
OJSC Plastic ABS 2020-31 ABS Plastic

POJSC962 / 192484

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.