MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC SABIC® LLDPE 518N PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: SABIC® LLDPE 518N is a butene linear low density polyethylene resin. Films produced from this resin have high toughness,good puncture resistance, good heat sealing behaviour and excellent machinability on conversion lines. Typical applications for SABIC® LLDPE518N are heavy duty shipping sacks, ice bags, frozen food bags, potato bags and agriculture films. Film properties: Film of 50 µm and BUR=2 has been produced on Kiefel IBC with 130 kg/h. Die size 200 mm, die gap 2,7 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D1505
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, TD 11.0 MPaISO 527-3
Film Elongation at Break, MD 550 %ISO 527-3
Film Elongation at Break, TD 800 %ISO 527-3
Tensile Modulus 170 MPaMD; ISO 527-3
 180 MPaTD; ISO 527-3
Puncture Energy 750 JJ/m; SABIC method
Tear Strength 30.0 kN/mMD; ISO 6383-2
 180 kN/mTD; ISO 6383-2
Dart Drop Total Energy 270 J/cmASTM D4272
Film Tensile Strength at Break, MD 40.0 MPaISO 527-3
Film Tensile Strength at Break, TD 32.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 120 °CSABIC method
Vicat Softening Point 104 °Cat 10 N (VST/A); ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 13 %ASTM D1003
Gloss 55 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11065 / 244532

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.