MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Akrochem Zinc Stearate
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Zinc Stearate is a clear-melting, high quality zinc carboxylate of stearic (C-18) and palmitic (C-16) acids that is ground to a very fine, highly dispersible white powder.

Applications: Zinc Stearate powder is an effective internal lubricant, mold release agent used in plastic processing and rubber applications. It is the metallic stearate of choice in most polyolefin processing applications due to its functionality and low moisture content. Zinc Stearate is an extremely heat stable product that is manufactured at low temperatures with minimal heat history. Zinc Stearate complies with FDA Standard CFR 21 sections 177.2600 and 178.2010.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
Particle Mesh Size 325 Mesh325 Mesh>95%
Ash 13 - 15 %13 - 15 %ZnO
 
Descriptive Properties
Appearancewhite powder
Content<1%Free Fatty Acid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH595 / 315513

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.