MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Resin Technology Group TIGA 920H Flexible Silver Conductive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 100 parts resin to 115 parts hardener.

TIGA 920-H is a flexible, conductive silver filled epoxy adhesive. It is recommended for bonding, and sealing electronic applications that require high flexibility, conductivity, and mechanical performance. This smooth paste formulation of pure silver and epoxy is free of solvents and extraneous additives. It develops strong, durable, electrically and thermally conductive bonds between many dissimilar materials including metals, ceramics and plastic laminates. TIGA 920-H cures at room temperature and can be used as a flexible “cold solder” for heat sensitive parts. It can also be used in the assembly and repair of flexible circuits, electrical components and electronic shielding.

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.90 g/cc2.90 g/cc
Solids Content 100 %100 %Reactive
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555
Shear Strength >= 3.45 MPa>= 500 psiLap, Au/Au
 >= 3.45 MPa>= 500 psiLap, Kaptona
 >= 6.89 MPa>= 1000 psiLap, Al/Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.0010 ohm-cm<= 0.0010 ohm-cmCured 2 hours at 65°C
 <= 0.0010 ohm-cm<= 0.0010 ohm-cmCured 1 hour at 110°C
 0.050 ohm-cm0.050 ohm-cmCured 12-24 hours at 25°C
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.55 W/m-K10.7 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 110 °C230 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 180 min
@Temperature 25.0 °C
180 min
@Temperature 77.0 °F
 
Descriptive Properties
ColorSilver
ViscositySmooth paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QSil 7750 Addition Cure, Thermally Conductive Material
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin
CENTROPLAST CENTROLYTE ZX Polyethylene terephthalate with lubricant
Bismuth, Bi
Avient Therma-Tech™ NNC-5000 TC Polyamide 66 (Nylon 66)

PRESINT604 / 65488

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.