MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil ExxonMobil™ PP1264E1 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: A high melt flow rate homopolymer resin designed to benefit large parts with long flow paths for appliance and other consumer products requiring long-term heat aging resistance.

Availability:  North America.  Features:  detergent resistant, heat aging resistant, thermal aging resistant, general purpose, heat stabilized, good processability, high flow.  Applications: appliance components, appliances, consumer applications.   Appearance:  natural color.  Forms: pellets.  Processing Method:  injection molding, compounding.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ExxonMobil Method
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 32.7 MPa4740 psi2.0 in/min; ASTM D638
Elongation at Yield 11 %11 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1290 MPa187000 psi0.051 in/min; ASTM D790A
 1480 MPa214000 psi0.51 in/min; ASTM D790B
Izod Impact, Notched 0.267 J/cm
@Temperature 22.8 °C
0.500 ft-lb/in
@Temperature 73.0 °F
ASTM D 256A
Izod Impact, Unnotched 1.39 J/cm
@Temperature -17.8 °C
2.60 ft-lb/in
@Temperature 0.000 °F
ASTM D256E
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.9 °C201 °Funannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C130 °Funannealed; ASTM D648
 
Descriptive Properties
Rockwell Hardness99ASTM D785

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEX98980 / 238361

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.