MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF 3-Amino-1-propanol
Categories: Fluid; Solvent

Material Notes: Formula: C3H9NO

CAS: 156-87-6

Description: 3-amino-1-propanol is a colorless to yellow liquid with an amine-like odor. It is miscible with water in all proportions.

Synonyms: Propanolamine, 3-aminopropanol, 3-Aminopropyl alcohol, 3-Hydroxy-1-aminopropane, 3-hydroxypropylamine,3-propanolamine

Applications: Intermediate used in the production of Pharmaceuticals, Cosmetics, Solvent, Electronics, Corrosion inhibitor and Synthetic resin & plasticize.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 - 0.990 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point 11.0 °C
Boiling Point 187 - 190 °C
Flash Point 101 °C
Ignition Temperature 375 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 0.50 %DIN 51 777
 
Descriptive Properties
Assay<99%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Piperazine Chips
BASF N-(3-Aminopropyl) imidazole
BASF Hexamethylenediamine
BASF AMIX 100

PBASG0852 / 132485

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.