MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC XENOY™ X5230 PC+PBT (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Mineral filled PC/PET blend with high flow, high heat, dimensional stability, low shrinkage and low CTE, especially for painted applications

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ISO 1183
Water Absorption 0.42 %0.42 %23°C/sat; ISO 62
Moisture Absorption 0.140 %0.140 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inSABIC method
Melt Flow  24 g/10 min
@Load 5.00 kg,
Temperature 265 °C
24 g/10 min
@Load 11.0 lb,
Temperature 509 °F
cm³/10 min; ISO 1133
 28 g/10 min
@Load 5.00 kg,
Temperature 265 °C
28 g/10 min
@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 42.0 MPa6090 psi5 mm/min; ISO 527
Tensile Strength, Yield 58.0 MPa8410 psi5 mm/min; ISO 527
Elongation at Break 9.0 %9.0 %5 mm/min; ISO 527
Elongation at Yield 3.6 %3.6 %5 mm/min; ISO 527
Tensile Modulus 3.85 GPa558 ksi1mm/min; ISO 527
Flexural Yield Strength 95.0 MPa13800 psi2 mm/min; ISO 178
Flexural Modulus 3.75 GPa544 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 137 kJ/m²65.2 ft-lb/in²80*10*4; ISO 180/1U
 120 kJ/m²
@Temperature -30.0 °C
57.1 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 54.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
30.0 µin/in-°F
@Temperature -22.0 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 74.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
41.1 µin/in-°F
@Temperature -22.0 - 176 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 109 °C228 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 137 °C279 °FRate B/50; ISO 306
 140 °C284 °FRate B/120; ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature
Nozzle Temperature 260 - 275 °C500 - 527 °FInjection Molding
Zone 1 240 - 270 °C464 - 518 °F
Zone 2 250 - 275 °C482 - 527 °F
Zone 3 260 - 280 °C500 - 536 °F
Melt Temperature 265 - 275 °C509 - 527 °F
Mold Temperature 60.0 - 100 °C140 - 212 °F
Drying Temperature 110 - 120 °C230 - 248 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Moisture Content 0.020 %0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10863 / 244330

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.