MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell DEXFLEX® 711 TPO  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: DEXFLEX® 711 is a thermoplastic olefinic elastomer compounded with post-industrial/post-consumer recycled materials. It is designed for use in applications that are (non-color matched) black, and that require very good processing characteristics.

Applications: Wheel liners, filler panels, fan shrouds, air dams, and sight shields

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccASTM D792
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM D995
Melt Flow 11 g/10 min11 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 19.0 MPa2760 psi50 mm/min, Type 4; ASTM D638
Flexural Modulus 0.860 GPa125 ksi0.05 in/min, 1x3"; ASTM D790
 
Thermal PropertiesMetricEnglishComments
CTE, linear 88.0 µm/m-°C
@Temperature 20.0 °C
48.9 µin/in-°F
@Temperature 68.0 °F
modified; ASTM D696

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Engineered Polymers Dexflex® 756-67 TPO
LyondellBasell DEXFLEX® 727 TPO
LyondellBasell Moplen HP550J Polypropylene Homopolymer
LyondellBasell DEXFLEX® 940 TPO
LyondellBasell DEXFLEX® 810-1 TPO

PSOLH11 / 68066

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.