Product Description: 90 Shore A TPE available in black and natural offering high heat performance with excellent oil and fluid resistance. This grade also exhibits high strength, good flexibility and resiliency. Intended for injection molding and extension processing. Designed for user the hood applications such as gaskets, grommets, seals, slugs where high heat and oil resistance is required. Availability: North America Features: Alcohol Resistant; Detergent Resistant; Good Adhesion; Good Colorability; Good Flexibility; Good Processability; High Elasticity; High Heat Resistance; High Strength; Low Compression Set; Oil Resistant; Ozone Resistant; Recyclable Material; Resilient; Soft; Solvent Resistant; UV Resistant Uses: Automotive Applications; Automotive Under the Hood; Gaskets; Grommets; Plugs; Seals Appearance: Black; Natural Color Processing Method: Extrusion; Injection Molding Information provided by Entec Polymers |